Does anyone know the revision letter and date for the specification AMS-S-13165??
I have looked in all of our books and on the internet. If anyone can help me find this please respond ASAP Thank you very much.
Paul Vanderkin

#416 12/08/99 04:19 PM
Joined: Apr 1999
Posts: 64
W
Member
OP Offline
Member
W
Joined: Apr 1999
Posts: 64
Paul,
No revision letter since this is NEW to SAE. Issue date is Nov 1997.

Cancellation date of MIL-S-13165C was 19 February 1998

Regards,
Jack Champaigne