Previous Thread
Next Thread
Print Thread
#538 08/26/99 09:18 AM
Joined: Jul 1999
Posts: 1
B
Bekink Offline OP
Member
OP Offline
Member
B
Joined: Jul 1999
Posts: 1
Considering the extreme expense of Zirblast Ceramic Beads in Europe a number of our customers are looking for an alternative abrasive.

The application is mainly to obtain an acceptable cosmetic effect on stainless steel equipment used in the food industry.

Also to clean welding seems etc.

Any suggestions would be welcom


Cees Bekink
Airblast BV
The Netherlands
[email protected]
www.airblast.com

#539 09/16/99 09:51 PM
Joined: May 1999
Posts: 200
Member
Offline
Member
Joined: May 1999
Posts: 200
We use #8 Glass (MILITARY GRADE) Bead to clean stainless steel weldments. Although glass beads don't come cheap they are less expensive then ceramic bead.