Hello Dr. Peener;

We have specified a Cast Steel Shot for our peenig material. I'm concerned about the residue that is left over after the peening procedure.

Do you have any information on the substance and amount of residue left over after peening?


Ron shillington
Joined: Apr 1999
Posts: 344
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 344
Likes: 1
Please download this paper from our library

http://www.shotpeening.org/ICSP/icsp-5-10.pdf