We manufacture light fixtures from 20 ga. stainless steel. We very much like the appearance of the glass bead blast finish. However we are having trouble with the material warping from the blasting. We tried turning down the pressure, but that just make it take longer to get the desired finish and it still warps. Do you have any suggestions short of using heavier material.


Jack Champaigne (Dr. Peener)
Editor The Shot Peener
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
What size of bead are you using? You might try a smaller glass bead size or ceramic bead.

Joined: Feb 2006
Posts: 3
D
Member
Offline
Member
D
Joined: Feb 2006
Posts: 3
Are you peening the fixture all over, or just on one side? If you are only peening one side, then peening the opposite side may cause shape recovery.


Daryll McKinley,
A Well-Worn Peening Enthusiast

Moderated by  Socrates 

Link Copied to Clipboard
Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5