We are developing an interesting approach to predict the high cycle fatigue performance of shot peened (two methods are developed: deterministic and probabilistic).

It can be used to optimise the shot peening conditions.

Also, an interesting FE model to predict the effects of shot peening on the surface conditions is developed.

If you are interested by a collaboration (applications of the developed methods), please do not hesitate to contact me.

raouf.fathallah@gmail.com


Prof. Raouf FATHALLAH
LGM - TUNISIA
www.lgm.rnu.tn
ENISo - TUNISIA
Joined: Feb 2009
Posts: 9
Y
Member
Offline
Member
Y
Joined: Feb 2009
Posts: 9
It is an interesting thing and I am interested in it. Could you give me the FE model? Thank you!


yukuigao
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
Prof FATHALLAH,
Please consider offering your work at the next International Conference on Shot Peening to be held in 2011. More information will be available soon at www.shotpeening.org.
Jack Champaigne
Chairman, ICSP-11