Hello can I please get help on shot peen blast of nichrome wire to clean it? This is a strand of wire about .010 DIA. It is self cleaned by heat to red hot. Thanks frankie

#98 01/19/09 02:50 AM
Joined: May 2005
Posts: 2
R
Member
Offline
Member
R
Joined: May 2005
Posts: 2
Could you please clarify process. Do you want to clean the wire ? What is the purpose of the heat treat ?


Ron Wright,
Wheelabrator Peening Products
[email protected]
#99 01/21/09 08:28 PM
Joined: Nov 2006
Posts: 4
F
frank Offline OP
Member
OP Offline
Member
F
Joined: Nov 2006
Posts: 4
Hello RON this is an o2 sensor for gas motors. the unit is cleaned after use with current to red hot. Thank You RON