Is there an SAE specification that details in depth how to perform correlation and peening of small holes with L/D<1? There seems to be many different opinions and ways of performing this but I cannot find a defined process.

Thanks

JAP #1238 07/28/16 01:06 PM
Joined: Apr 1999
Posts: 344
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 344
Likes: 1
Nothing in SAE specs but this article from Progressive may help.

http://www.shotpeener.com/library/detail.php?anc=2003005&keyword=barker

JAP #1239 07/28/16 03:05 PM
Joined: Mar 2016
Posts: 10
J
JAP Offline OP
Member
OP Offline
Member
J
Joined: Mar 2016
Posts: 10
Is there any reason not to correlate directly from a standard strip to a hole test? I have also read about an R2 value but not sure what this is.

It would be good to get a standardized process across the industry but thanks for the info Jack.


Link Copied to Clipboard
Sponsored by Electronics Inc. © 2025 Electronics Inc. All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5