Hi, is it ok to use m5 allen key bolt instead of the pan head type described in j442 ? " Use pan head (or smaller head diameter) style screw of size M5."

The allen key bolt has a smaller head than a pan head.

/R

google search bolt Picture


Shotpeen Engineer
Joined: Apr 2011
Posts: 56
Likes: 1
Member
Offline
Member
Joined: Apr 2011
Posts: 56
Likes: 1
Changing the head type is fine as long as the head isn't larger, thus causing an excessive "shaded" area.

EI uses hex (Allen) screws in their products. Recently I heard someone report that star (Torx) heads have a longer life span than hex style.


Dave Barkley
EI SPT Director, Peening Preceptor & Product Engineer
Joined: Nov 2013
Posts: 10
B
Member
OP Offline
Member
B
Joined: Nov 2013
Posts: 10
The heads height is not defined in the spec. Is it then ok to use the cylindrical bolts that I linked to as long as the diameter is smaller than a typical pan head and its not leaving an excessive shade ?
I think the hex or torx is muche more user friendly as you say.


Shotpeen Engineer
Joined: Apr 2011
Posts: 56
Likes: 1
Member
Offline
Member
Joined: Apr 2011
Posts: 56
Likes: 1
Just be careful of heads that are too tall, as they can shade when the blast stream comes in at lower angles. wink


Dave Barkley
EI SPT Director, Peening Preceptor & Product Engineer

Link Copied to Clipboard