Newby question alert....

So I perform the saturation curves prior to a new job/parameters. Then from that day forward anytime we do that job running to the set parameters at the beginning of the job I perform a an arc height verification and then I perform another when the job is complete - even if that is 2 days later.

First question: Is this the right approach?
Second question: Is there a standardized Inspection form for this process? no sense in reinventing the wheel if their is a form someone has created for capturing this information already - to include prebow measurements and prebow comp.

Joined: Apr 2019
Posts: 18
R
Rich Offline OP
Member
OP Offline
Member
R
Joined: Apr 2019
Posts: 18
Question to admins. After 212 views I receive no response. Have I posted my question in the wrong section and/or forum?

Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
I would consider the process you are using as being correct.
However, the frequency of verifications has never been a part of SAE specs since it is considered to be part of the companies quality assurance program.
I am not aware of any standard forms. Again, these do not exist in any SAE document since every company would have its own requirements.
You are welcome to attend our SAE meetings. The next meeting is May 5, 2020 in Troy Michigan. Contact me if you would like to attend. Jack.champaigne@electronics-inc.com

Joined: Feb 2006
Posts: 112
S
Member
Offline
Member
S
Joined: Feb 2006
Posts: 112
Solver programs allow for pre-bow and pre-bow compensation.