What is the best position of almen strip for intensity verification, horizontal or vertical? The case is shaded almen strip, representing small blade slots. I ask because sometimes I see the strip positioned vertically, although in my opinion it should be horizontally.
Thank you in advance.

Y.S. #1547 08/09/21 02:48 PM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
You should choose an orientation that best represents your peening setup. Without photos, it isn't easy to give any more advice.