Previous Thread
Next Thread
Print Thread
#1604 01/16/23 04:03 PM
Joined: Jan 2023
Posts: 3
B
BenM Offline OP
Member
OP Offline
Member
B
Joined: Jan 2023
Posts: 3
Hello All,

We're occasionally asked if we're able to provide the WPC process. The answer has always been 'no' but I'd like to learn more about it.

Does anybody have any experience of the process?

I understand the process to involve 'high velocity' peening using a mix of steel shot smaller than the ASH range, but I don't understand exactly how the process is defined/controlled.

Is the process licenced? Does it require any special equipment (beyond the media), or is it possible with a conventional pressure blast cabinet machine?

I'd be keen to hear if anybody has any first hand experience of the process, and if anybody could point me in the right direction to find out more.

Thanks

Ben

BenM #1605 01/16/23 04:11 PM
Joined: May 1999
Posts: 202
Member
Offline
Member
Joined: May 1999
Posts: 202
Perhaps this company can help you. https://wpctreatment.com/about.htm

BenM #1606 01/16/23 05:27 PM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1

BenM #1607 01/16/23 05:44 PM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
Here is another article of interest:

https://www.shotpeener.com/library/detail.php?anc=2016029&keyword=%22wpc+treatment%22

BenM #1608 01/30/23 12:27 PM
Joined: Jan 2023
Posts: 3
B
BenM Offline OP
Member
OP Offline
Member
B
Joined: Jan 2023
Posts: 3
Thank you both for your comments, very educational. It appears it's not licenced/available outside of Japan/US.
We're based in the UK, so I guess we will stick to good old fashioned shot peening for the time being!

BenM #1609 01/30/23 04:01 PM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
The US patent 5,592,840 June 14, 1997 Method of preventing abrasion at sliding portion of metal-product has lapsed. No license is needed after expiration.