The knowledge base for the shot peening and blast cleaning industries
≡
About
The Website
Shot Peening
Library
Search the Library
Recently added articles
The Shot Peener
articles
Dr. David Kirk articles
Dr. John Cammett articles
Patents Granted
Patent Applications
Specifications
FAQs
Shot Peener of the Year
Wheelabrator History
Vacu-Blast History
Pangborn History
Jack's History Finds
Tools
Almen Saturation Curve Solver Program
Peening Coverage Predictor Program
Two-Strip Intensity Estimator
Program Request Form
Vibrator Screen Check Decal
Shot Peening Saturation Curve Practice Sheet
Roto-Flap Peening Saturation Curve Practice Sheet
Charts and graphs
Intensity as function of shot size for wheel peening
Sweco screen sizes for sand blasting and shot peening media
Vacu-Blast Engineering Specifications - Nozzle Performance
Buyer's Guide
Vendors
Products
Register company
Q & A Forum
News
Contact
Register
Log In
Home
Forums
General Discussion
Shot Peening Process, Intensity, Coverage
Conditioning New Cast Steel Shot
Forums
Active Threads
Previous Thread
Next Thread
Print Thread
Re: Conditioning New Cast Steel Shot
#
11
04/09/10
09:10 PM
Joined:
May 1999
Posts: 202
East Hartford, CT, USA
Walter
Member
Walter
Member
Joined:
May 1999
Posts: 202
East Hartford, CT, USA
Is your air pressure tolerance really +/- 10 PSI? If so that may very well be your problem.
I would suggest you change your air pressure limits to +/-10% from nominal across the board on all your machines.
Copy Link to Clipboard
Entire Thread
Subject
Posted By
Posted
Conditioning New Cast Steel Shot
Gary J
04/07/10
06:50 PM
Re: Conditioning New Cast Steel Shot
Lennart Almqvist
04/08/10
01:46 PM
Re: Conditioning New Cast Steel Shot
Walter
04/08/10
02:00 PM
Re: Conditioning New Cast Steel Shot
Gary J
04/08/10
06:57 PM
Re: Conditioning New Cast Steel Shot
Pete Bailey
04/08/10
07:21 PM
Re: Conditioning New Cast Steel Shot
Walter
04/08/10
08:24 PM
Re: Conditioning New Cast Steel Shot
Socrates
04/08/10
08:46 PM
Re: Conditioning New Cast Steel Shot
Joe McGreal
04/08/10
08:55 PM
Re: Conditioning New Cast Steel Shot
Gary J
04/09/10
06:41 PM
Re: Conditioning New Cast Steel Shot
Walter
04/09/10
08:51 PM
Re: Conditioning New Cast Steel Shot
Walter
04/09/10
09:10 PM
Re: Conditioning New Cast Steel Shot
Joe McGreal
04/12/10
01:39 PM
Re: Conditioning New Cast Steel Shot
Alberto Rodriguez
04/12/10
03:29 PM
Re: Conditioning New Cast Steel Shot
Gary J
04/13/10
06:59 PM
Re: Conditioning New Cast Steel Shot
Marcel vW
07/05/10
02:36 PM
Moderated by
Andy Levers
,
Dave Barkley
,
Jack Champaigne
,
Jeff Derda
,
John Cammett
,
Kumar Balan
,
Socrates
,
Walter
Hop To
General Discussion ------
Shot Peening Process, Intensity...
Specifications
Equipment, Machines, Accessories
Abrasive Blast Cleaning Process
Media, Shot, Beads, etc.
Ask Dr. Peener
Print Thread
Switch to Flat Mode
Show Likes
Link Copied to Clipboard
View Profile
Private Message
Website
Follow User
Forum Posts
Like Summary
Forum Rules
·
Mark All Read
Contact Us
·
Forum Help
·
Home
Sponsored by Electronics Inc. © 2026
Electronics Inc.
All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5