Forwarded response from Herb Tobben at Clemco:
Hi Jack Champaigne,
This is unusual, I do not recall ever working with a Shot Peening application using S-780 shot.
S-550 shot is the largest that I recall using for Shot Peening.
The lance would have to be special made, I would suggest starting with a minimum of one half inch I. D.
Herb Tobben