Just recently received a customer request for LAT4-0214 spec. Many years in this industry and I have never encounter this spec before. Any help would greatly be appreciated

Newf #1188 11/18/15 12:38 PM
Joined: Nov 2015
Posts: 4
F
Member
Offline
Member
F
Joined: Nov 2015
Posts: 4
Hi the spec it a Liebherr specification, Glass Bead (Bright Shot) Peening for Bombardier