I am setting up a small QC area to analysis the surface of blasted metals. I'll be blasting the part or strip in the cabinet, then looking how the surface finish changed. Is there a recommended profilometer(with computer connectivity) that is widely used by this industry? I saw some handheld devices that were around $4000. I want to keep price down as my budget is tight, but I'd like to use equipment that is widely recognized in the metal finishing/peening arena so potential customers are more comfortable with the data produce.
Any suggestions would be great!

Thanks!

Joined: Sep 2014
Posts: 16
C
Member
Offline
Member
C
Joined: Sep 2014
Posts: 16
I recommend the SJ-210 series by Mitutoyo. Its not cheap at about $2500 but it is a good piece of equipment. Computer connectivity is something I am not sure about, but it has its own LCD screen with data logging capability and roughness charts. Many of our aerospace customers also use this profilometer in their inspection areas.

Last edited by Charlie; 05/17/16 07:44 PM.

Link Copied to Clipboard
Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5