The knowledge base for the shot peening and blast cleaning industries
≡
About
The Website
Shot Peening
Library
Search the Library
Recently added articles
The Shot Peener
articles
Dr. David Kirk articles
Dr. John Cammett articles
Patents Granted
Patent Applications
Specifications
FAQs
Shot Peener of the Year
Wheelabrator History
Vacu-Blast History
Pangborn History
Jack's History Finds
Tools
Almen Saturation Curve Solver Program
Peening Coverage Predictor Program
Two-Strip Intensity Estimator
Program Request Form
Vibrator Screen Check Decal
Shot Peening Saturation Curve Practice Sheet
Roto-Flap Peening Saturation Curve Practice Sheet
Charts and graphs
Intensity as function of shot size for wheel peening
Sweco screen sizes for sand blasting and shot peening media
Vacu-Blast Engineering Specifications - Nozzle Performance
Buyer's Guide
Vendors
Products
Register company
Q & A Forum
News
Contact
Register
Log In
Home
Forums
General Discussion
Specifications
AMS2430 Appendix A.2.2.6.5 Specimen Material Query
Forums
Active Threads
Previous Thread
Next Thread
Print Thread
AMS2430 Appendix A.2.2.6.5 Specimen Material Query
#
1530
04/29/21
07:12 AM
Joined:
Mar 2021
Posts: 9
Likes: 1
United Kingdom
V
Very Old Tom
OP
Member
OP
Very Old Tom
Member
V
Joined:
Mar 2021
Posts: 9
Likes: 1
United Kingdom
How critical is the steel material properties for the operator qualification specimens. Is it permitted to use a steel alloy with a lower than 180 to 300 ksi UTS condition ?
Copy Link to Clipboard
Entire Thread
Subject
Posted By
Posted
AMS2430 Appendix A.2.2.6.5 Specimen Material Query
Very Old Tom
04/29/21
07:12 AM
Re: AMS2430 Appendix A.2.2.6.5 Specimen Material Query
Walter
04/30/21
01:59 PM
Re: AMS2430 Appendix A.2.2.6.5 Specimen Material Query
BenM
09/20/23
04:03 PM
Moderated by
Andy Levers
,
Dave Barkley
,
Jack Champaigne
,
Jeff Derda
,
John Cammett
,
Kumar Balan
,
Socrates
,
Walter
Hop To
General Discussion ------
Shot Peening Process, Intensity...
Specifications
Equipment, Machines, Accessories
Abrasive Blast Cleaning Process
Media, Shot, Beads, etc.
Ask Dr. Peener
Print Thread
Switch to Flat Mode
Show Likes
Link Copied to Clipboard
View Profile
Private Message
Follow User
Forum Posts
Like Summary
Forum Rules
·
Mark All Read
Contact Us
·
Forum Help
·
Home
Sponsored by Electronics Inc. © 2026
Electronics Inc.
All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5