The knowledge base for the shot peening and blast cleaning industries
≡
About
The Website
Shot Peening
Library
Search the Library
Recently added articles
The Shot Peener
articles
Dr. David Kirk articles
Dr. John Cammett articles
Patents Granted
Patent Applications
Specifications
FAQs
Shot Peener of the Year
Wheelabrator History
Vacu-Blast History
Pangborn History
Jack's History Finds
Tools
Almen Saturation Curve Solver Program
Peening Coverage Predictor Program
Two-Strip Intensity Estimator
Program Request Form
Vibrator Screen Check Decal
Shot Peening Saturation Curve Practice Sheet
Roto-Flap Peening Saturation Curve Practice Sheet
Charts and graphs
Intensity as function of shot size for wheel peening
Sweco screen sizes for sand blasting and shot peening media
Vacu-Blast Engineering Specifications - Nozzle Performance
Buyer's Guide
Vendors
Products
Register company
Q & A Forum
News
Contact
Register
Log In
Home
Forums
General Discussion
Shot Peening Process, Intensity, Coverage
Media max intensity
Forums
Active Threads
Previous Thread
Next Thread
Print Thread
Re: Media max intensity
JAP
#
1583
06/01/22
07:04 PM
Joined:
Apr 2011
Posts: 56
Likes: 1
USA
Dave Barkley
Member
Dave Barkley
Member
Joined:
Apr 2011
Posts: 56
Likes: 1
USA
I will usually refer to
THIS TABLE
to get a generic idea of what intensity each size of cast steel shot can achieve.
Perhaps Table 4 from ARP7488 can be extrapolated to determine the potential of other media types.
Dave Barkley
EI SPT Director, Peening Preceptor & Product Engineer
1 member likes this
:
JAP
Copy Link to Clipboard
Entire Thread
Subject
Posted By
Posted
Media max intensity
JAP
05/24/22
02:18 PM
Re: Media max intensity
Dave Barkley
06/01/22
07:04 PM
Moderated by
Andy Levers
,
Dave Barkley
,
Jack Champaigne
,
Jeff Derda
,
John Cammett
,
Kumar Balan
,
Socrates
,
Walter
Hop To
General Discussion ------
Shot Peening Process, Intensity...
Specifications
Equipment, Machines, Accessories
Abrasive Blast Cleaning Process
Media, Shot, Beads, etc.
Ask Dr. Peener
Print Thread
Switch to Flat Mode
Show Likes
Link Copied to Clipboard
View Profile
Private Message
Website
Follow User
Forum Posts
Like Summary
Forum Rules
·
Mark All Read
Contact Us
·
Forum Help
·
Home
Sponsored by Electronics Inc. © 2026
Electronics Inc.
All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5