Previous Thread
Next Thread
Print Thread
Joined: Aug 2016
Posts: 20
D
donhan Offline OP
Member
OP Offline
Member
D
Joined: Aug 2016
Posts: 20
Hello All,

Our shot peening machine equipped with Magna Valve 578-24.

Our customer requires to shot part with SST-54-CW SHOT.

Could you please advise if magna valve is able to work with SST-54-CW SHOT ?

Thanks a lot.

Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
I am not familiar with SST-54 CW shot. Can you send me a copy of the specification?
You may send information to scott.harvey@electronics-inc.com

Joined: May 1999
Posts: 202
Member
Offline
Member
Joined: May 1999
Posts: 202
I believe Dohan wants to know if the 578-24 will work with Stainless Steel Conditioned Cut Wire peening media.

Joined: Aug 2016
Posts: 20
D
donhan Offline OP
Member
OP Offline
Member
D
Joined: Aug 2016
Posts: 20
Dear Jack,

Actually, I also don't have the specific specification for SST-54 CW. But as Walter said that is right, Stainless Steel Conditioned Cut Wire size 54 is the shot i want to say. The drawing only specify the name SST-54-CW shots and general spec MIL-S-851.

Hope this can help you to advise me to explore somethings on it.

Thanks


Link Copied to Clipboard
Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5