The knowledge base for the shot peening and blast cleaning industries
≡
About
The Website
Shot Peening
Library
Search the Library
Recently added articles
The Shot Peener
articles
Dr. David Kirk articles
Dr. John Cammett articles
Patents Granted
Patent Applications
Specifications
FAQs
Shot Peener of the Year
Wheelabrator History
Vacu-Blast History
Pangborn History
Jack's History Finds
Tools
Almen Saturation Curve Solver Program
Peening Coverage Predictor Program
Two-Strip Intensity Estimator
Program Request Form
Vibrator Screen Check Decal
Shot Peening Saturation Curve Practice Sheet
Roto-Flap Peening Saturation Curve Practice Sheet
Charts and graphs
Intensity as function of shot size for wheel peening
Sweco screen sizes for sand blasting and shot peening media
Vacu-Blast Engineering Specifications - Nozzle Performance
Buyer's Guide
Vendors
Products
Register company
Q & A Forum
News
Contact
Register
Log In
Home
Forums
General Discussion
Shot Peening Process, Intensity, Coverage
Convert Almen A Results to Almen C
Forums
Active Threads
Previous Thread
Next Thread
Print Thread
Re: Convert Almen A Results to Almen C
Jean Riesling
#
1627
03/28/24
03:39 PM
Joined:
May 1999
Posts: 202
East Hartford, CT, USA
Walter
Member
Walter
Member
Joined:
May 1999
Posts: 202
East Hartford, CT, USA
Jean,
The conversion factor is for refence only. You are not permitted to use a different strip scale than what is called out on the engineering drawing.
Copy Link to Clipboard
Entire Thread
Subject
Posted By
Posted
Convert Almen A Results to Almen C
tec
07/22/14
01:23 PM
Re: Convert Almen A Results to Almen C
Socrates
07/22/14
02:21 PM
Re: Convert Almen A Results to Almen C
Jean Riesling
03/28/24
02:33 PM
Re: Convert Almen A Results to Almen C
Walter
03/28/24
03:39 PM
Moderated by
Andy Levers
,
Dave Barkley
,
Jack Champaigne
,
Jeff Derda
,
John Cammett
,
Kumar Balan
,
Socrates
,
Walter
Hop To
General Discussion ------
Shot Peening Process, Intensity...
Specifications
Equipment, Machines, Accessories
Abrasive Blast Cleaning Process
Media, Shot, Beads, etc.
Ask Dr. Peener
Print Thread
Switch to Flat Mode
Show Likes
Link Copied to Clipboard
View Profile
Private Message
Website
Follow User
Forum Posts
Like Summary
Forum Rules
·
Mark All Read
Contact Us
·
Forum Help
·
Home
Sponsored by Electronics Inc. © 2026
Electronics Inc.
All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5