Thank you very much Walter!
interesting answer
For drawing a type 2 saturation curve, I would still need much homogenuous result, isn'it? Here I clearly have the iconic rise of a type 1 saturation curve at the begining confused
If test strip is 100% covered, and max residual stress is obtained at 100% coverage, what mechanism make the almen plate continue to bend? recrystalisation? Almen plate is already made out of hard material and fine structure.