Our company, Standen's Limited, is involved in the manufacture of heat treated spring steel products, mainly springs and agricultural products, a great deal of which are shot or stress peened. As such, we generate large amounts of shot peen dust off of our cast S660 shot. Does any of you presently sell your shot peen dust? If so, who buys this byproduct? Or do any of you purchase this material?
I look forward to hearing from you...THANKS.
Philip Lockey

Standen's Limited

1222 58th Avenue S.E.

Calgary, Alberta, Canada
T2H 2G7

Ph: 403-258-7800 ext. 755

Fax: 403-258-7808

philip.lockey@standens.com

#167 12/27/04 05:56 PM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
Contact GMA Industries at their web site:
http://www.gmaind.com/


Link Copied to Clipboard
Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5