I'd like to know what device/container is habitually used to perform catch tests?

#174 07/07/06 02:17 PM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
I know of three companies that make special catch test devices:
Mike Wern
President
Engineered Abrasives
11631 South Austin Avenue
Alsip, IL 60803 USA
(708)389-9700
http://www.engineeredabrasives.com

Jim Whalen
VP Sales & Marketing
Progressive Technologies
4201 Patterson Ave. Street SE
Grand Rapids, MI 49512-4033 USA
(616)957-0871

Dominique Schwab
General Manager
Sisson Lehmann Wheelabrator Group
24 rue Camille Didier BP 39
Charleville-Mézières Cédex, F-08001 FRANCE
33-324-336319


Link Copied to Clipboard
Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5