The knowledge base for the shot peening and blast cleaning industries
≡
About
The Website
Shot Peening
Library
Search the Library
Recently added articles
The Shot Peener
articles
Dr. David Kirk articles
Dr. John Cammett articles
Patents Granted
Patent Applications
Specifications
FAQs
Shot Peener of the Year
Wheelabrator History
Vacu-Blast History
Pangborn History
Jack's History Finds
Tools
Almen Saturation Curve Solver Program
Peening Coverage Predictor Program
Two-Strip Intensity Estimator
Program Request Form
Vibrator Screen Check Decal
Shot Peening Saturation Curve Practice Sheet
Roto-Flap Peening Saturation Curve Practice Sheet
Charts and graphs
Intensity as function of shot size for wheel peening
Sweco screen sizes for sand blasting and shot peening media
Vacu-Blast Engineering Specifications - Nozzle Performance
Buyer's Guide
Vendors
Products
Register company
Q & A Forum
News
Contact
Register
Log In
Home
Forums
General Discussion
Shot Peening Process, Intensity, Coverage
shot peening of single crystal
Forums
Active Threads
Previous Thread
Next Thread
Print Thread
shot peening of single crystal
#
229
02/07/09
03:08 PM
Joined:
Feb 2009
Posts: 9
Beijing
Y
Yu-kui GAO
OP
Member
OP
Yu-kui GAO
Member
Y
Joined:
Feb 2009
Posts: 9
Beijing
Many metals are shot peening to modify fatigue, SCC and fretting ect. properties, especially for polycrystallines. How about shot peening of single crystals? Thank you for your kind advice in advance on this topic.
yukuigao
Copy Link to Clipboard
Entire Thread
Subject
Posted By
Posted
shot peening of single crystal
Yu-kui GAO
02/07/09
03:08 PM
Re: shot peening of single crystal
Pete Bailey
02/07/09
06:07 PM
Re: shot peening of single crystal
Yu-kui GAO
02/08/09
12:42 PM
Moderated by
Andy Levers
,
Dave Barkley
,
Jack Champaigne
,
Jeff Derda
,
John Cammett
,
Kumar Balan
,
Socrates
,
Walter
Hop To
General Discussion ------
Shot Peening Process, Intensity...
Specifications
Equipment, Machines, Accessories
Abrasive Blast Cleaning Process
Media, Shot, Beads, etc.
Ask Dr. Peener
Print Thread
Switch to Flat Mode
Show Likes
Link Copied to Clipboard
View Profile
Private Message
Follow User
Forum Posts
Like Summary
Forum Rules
·
Mark All Read
Contact Us
·
Forum Help
·
Home
Sponsored by Electronics Inc. © 2026
Electronics Inc.
All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5