I have a customer that would like me to shot peen some impellers. The specification is 6 to 10 A intensity with 110 shot 125% coverage.

I would need to do this with a suction blaster. Can I acheive these results with a suction blaster?

I understand that I would need the Almen strips and fixturing to set up process parameters, but before purchasing this I would like to know first if it is even possible.

Any other tips on things to consider would be appreciated.

Thanks very much.

Joined: Apr 1999
Posts: 344
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 344
Likes: 1
The answer is "probably yes". If you have adequate air pressure and a good nozzle design. You should consult with several machine manufactures in advance, they can provide a set up to prove the capability in advance.