I would like to know if unsymmetrical setting of the Almen strip will affect the intensety. I mean that there is shaded areas but thay are not even on the strip.
Is there a spesification thet demends symmetrical shades?


Shlomi Kisluk
Bedek-Engines Div. Material & Process Engineering
ISRAEL AEROSPACE INDUSTRIES
972-3-9358300
972-52-6040517
#240 09/25/03 11:56 PM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
I don't understand your question. What do you mean by "shaded" areas on the strip? The strip is supposed to be uniformly and completely covered by the peening treatment. Can you supply an image of a strip you are referring to?

#241 09/26/03 05:39 AM
Joined: May 2003
Posts: 7
kisluk Offline OP
Member
OP Offline
Member
Joined: May 2003
Posts: 7
I mean Shaded by the boltes that hold the strip.


Shlomi Kisluk
Bedek-Engines Div. Material & Process Engineering
ISRAEL AEROSPACE INDUSTRIES
972-3-9358300
972-52-6040517
#242 10/02/03 02:32 PM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
The un-peened area underneath the bolt heads can be ignored. These areas do not have to be peened and will be shaded. This is standard practice, nothing to worry about.