Jack:

We're looking into media blasting for stripping paint from aluminum wheels.
We will need an automated system with a plastic, steel shot, or glass
media. What should I be looking for in a system and what are the pros and
cons of the different media?
Thanks.
Keith

#306 05/20/03 12:13 AM
Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
OP Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
Keith,
The different media will have different levels of aggressiveness. Plastic, as well as wheat starch and bicarbonate of soda, will be gentle, glass will leave a sheen, steel shot may leave ferrous contamination (rust).

When you say "automatic system", what level of automation are you considering? Or better yet, what quantity of wheels do you need to process? Do you plan to build your own machine or purchase? You can use air blast for high velocity blast (small quantities of wheels) or wheel blast system for high volume of media and high quantities of wheels to blast.
You might consider using a contract job shop at first to refine your process or seek a machine builder that can do small quantity production during your development program.

Jack