What will be the best way to store an Almen jig to prevent corrosion? What is commontly use? confused

Joined: May 1999
Posts: 200
Member
Offline
Member
Joined: May 1999
Posts: 200
We spray the almen holders with dyekm blue. Works well and has stood up to Nadcap inspection.