I am going to simulate the Almen test process with finite element method. Is there anybody have more material properties of Almen strip, such as yield stress, tangent modulus, or the stress-stain relationship of Almen strip at high speed strain, ect. Thanks!

#371 09/15/08 07:22 AM
Joined: Sep 2007
Posts: 11
D
Member
Offline
Member
D
Joined: Sep 2007
Posts: 11
As per SAE J442 the strips are made of SAE 1070 colled rolled spring steel. Some properties are given at the following website:
http://www.substech.com/dokuwiki/doku.ph...4368a3950673cc5

Perhaps the values given there are sufficient for a FE model.