Dear Jack,
We use the Almen strip block for our shot peen process and some of our Almen blocks are worn and old and in need of sorting.
Can you please let me know?
What is a bridge gage?
What is the best way to check the Almen block flatness?
How do you check it?

Thanks in advance


Jack Champaigne (Dr. Peener)
Editor The Shot Peener
#374 01/07/05 04:20 PM
Joined: Jan 2005
Posts: 35
Administrator
OP Offline
Administrator
Joined: Jan 2005
Posts: 35
The Almen blocks can be re-surfaced by grinding to get the surface flat again.

The surface should then be checked with a dial indicator for flatness.
There is presently a tolerance for flatness of 0.1mm according to SAE J442.
You can also submit the holder to a lapping machine for further confidence.

I am not familiar with the term bridge gage.


Jack Champaigne (Dr. Peener)
Editor The Shot Peener

Link Copied to Clipboard
Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5