I would like to try using a fluorescent tracer to verify peening coverage. I am having problems finding suppliers. Anyone out there have any supplier contact information it would be greatly appreciated. Thank you in advance, Scott

Joined: Apr 1999
Posts: 344
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 344
Likes: 1
A product called Fluro-Finder is available at Electronics Inc.