Hi!
At AMS-S-13165 table VI "Shot Peening Intensity" the
steel is classified as under 200000psi and over
200000psi. Is this the Ultimate tensile strenth or
the Yield Strenth of the material?

#413 07/10/07 07:41 PM
Joined: Apr 1999
Posts: 344
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 344
Likes: 1
It is the Ultimate Tensile Strength