The knowledge base for the shot peening and blast cleaning industries
≡
About
The Website
Shot Peening
Library
Search the Library
Recently added articles
The Shot Peener
articles
Dr. David Kirk articles
Dr. John Cammett articles
Patents Granted
Patent Applications
Specifications
FAQs
Shot Peener of the Year
Wheelabrator History
Vacu-Blast History
Pangborn History
Jack's History Finds
Tools
Almen Saturation Curve Solver Program
Peening Coverage Predictor Program
Two-Strip Intensity Estimator
Program Request Form
Vibrator Screen Check Decal
Shot Peening Saturation Curve Practice Sheet
Roto-Flap Peening Saturation Curve Practice Sheet
Charts and graphs
Intensity as function of shot size for wheel peening
Sweco screen sizes for sand blasting and shot peening media
Vacu-Blast Engineering Specifications - Nozzle Performance
Buyer's Guide
Vendors
Products
Register company
Q & A Forum
News
Contact
Register
Log In
Home
Forums
General Discussion
Specifications
"Edge Type: Number 1" in J442
Forums
Active Threads
Previous Thread
Next Thread
Print Thread
"Edge Type: Number 1" in J442
#
425
01/05/07
02:39 PM
Joined:
Jan 2007
Posts: 2
Cincinnati, OH
J
John Z
OP
Member
OP
John Z
Member
J
Joined:
Jan 2007
Posts: 2
Cincinnati, OH
J442 specifies a number 1 edge on the 3" side of Almen strips. Can anyone tell me what industry spec governs exactly what consitutes an acceptable number 1 edge?
Thanks,
John Z.
Copy Link to Clipboard
Entire Thread
Subject
Posted By
Posted
"Edge Type: Number 1" in J442
John Z
01/05/07
02:39 PM
Re: "Edge Type: Number 1" in J442
Jack Champaigne
01/05/07
03:42 PM
Re: "Edge Type: Number 1" in J442
John Z
01/09/07
03:27 PM
Moderated by
Andy Levers
,
Dave Barkley
,
Jack Champaigne
,
Jeff Derda
,
John Cammett
,
Kumar Balan
,
Socrates
,
Walter
Hop To
General Discussion ------
Shot Peening Process, Intensity...
Specifications
Equipment, Machines, Accessories
Abrasive Blast Cleaning Process
Media, Shot, Beads, etc.
Ask Dr. Peener
Print Thread
Switch to Flat Mode
Show Likes
Link Copied to Clipboard
View Profile
Private Message
Follow User
Forum Posts
Like Summary
Forum Rules
·
Mark All Read
Contact Us
·
Forum Help
·
Home
Sponsored by Electronics Inc. © 2025
Electronics Inc.
All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5