The knowledge base for the shot peening and blast cleaning industries
≡
About
The Website
Shot Peening
Library
Search the Library
Recently added articles
The Shot Peener
articles
Dr. David Kirk articles
Dr. John Cammett articles
Patents Granted
Patent Applications
Specifications
FAQs
Shot Peener of the Year
Wheelabrator History
Vacu-Blast History
Pangborn History
Jack's History Finds
Tools
Almen Saturation Curve Solver Program
Peening Coverage Predictor Program
Two-Strip Intensity Estimator
Program Request Form
Vibrator Screen Check Decal
Shot Peening Saturation Curve Practice Sheet
Roto-Flap Peening Saturation Curve Practice Sheet
Charts and graphs
Intensity as function of shot size for wheel peening
Sweco screen sizes for sand blasting and shot peening media
Vacu-Blast Engineering Specifications - Nozzle Performance
Buyer's Guide
Vendors
Products
Register company
Q & A Forum
News
Contact
Register
Log In
Home
Forums
General Discussion
Media, Shot, Beads, etc.
What to use/ how to specify?
Forums
Active Threads
Previous Thread
Next Thread
Print Thread
Re: What to use/ how to specify?
#
551
07/26/99
01:06 PM
Joined:
Jul 1999
Posts: 1
Boardman,Oh,USA
M
Marlac
Member
Marlac
Member
M
Joined:
Jul 1999
Posts: 1
Boardman,Oh,USA
If you need to prep without a profile then you have a rather tuff task. There is only one company that can prep without a profile.
call 330-965-0071 ask for Dean
Copy Link to Clipboard
Entire Thread
Subject
Posted By
Posted
What to use/ how to specify?
pharan
06/23/99
01:21 PM
Re: What to use/ how to specify?
Marlac
07/26/99
01:06 PM
Moderated by
Andy Levers
,
Dave Barkley
,
Dennis Scharer
,
Jack Champaigne
,
Jeff Derda
,
John Cammett
,
Kumar Balan
,
Socrates
,
Walter
Hop To
General Discussion ------
Shot Peening Process, Intensity...
Specifications
Equipment, Machines, Accessories
Abrasive Blast Cleaning Process
Media, Shot, Beads, etc.
Ask Dr. Peener
Print Thread
Switch to Flat Mode
Show Likes
Link Copied to Clipboard
View Profile
Private Message
Website
Follow User
Forum Posts
Like Summary
Forum Rules
·
Mark All Read
Contact Us
·
Forum Help
·
Home
Sponsored by Electronics Inc. © 2025
Electronics Inc.
All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5