Hello-
We are interested in having re-manufactured or reclaimed steel shot tested for durability and hardness. Is there a 3rd party capable of providing this service? Appreciate any insight.

Jay Lenick
Atwater Steel Trading Corporation
Pittsburgh, PA
412-310-5586 (m)


AtwaterSteel
Joined: Jan 2011
Posts: 3
L
Member
Offline
Member
L
Joined: Jan 2011
Posts: 3
Our company can provide this service test ,we have the machine.if you need ,just write to me ,lanelau@hotmail.com