Dear Jack,
We are searching for suppliers of Black Beauty for distribution
purposes. Could you send us a list of this material?
You may like to know we are wholesale distributors for Graco, Binks,
Clemco, Quincy and many other good manufacturers.
Many thanks for your kind courtesies.
Neville Hobson-Garcia
Paints and Equipment Limited
51, Tragarete Road,
P.O. Box 34,
Port of Spain.
Trinidad W.I.
Tel: (868) 628-7501/ 0508/ 0507
Fax: (868) 628-2114

paintequ@tstt.net.tt

[Note: This message has been edited by webmaster]


[Note: This message has been edited by webmaster]

Joined: Apr 1999
Posts: 345
Likes: 1
J
Member
Offline
Member
J
Joined: Apr 1999
Posts: 345
Likes: 1
Dear Neville,
I have heard of Black Beauty and know that it exists but do not know who
might distribute it. Perhaps some of our readers can help.
Regards,
Jack

Joined: Apr 1999
Posts: 64
W
Member
OP Offline
Member
W
Joined: Apr 1999
Posts: 64
Black Beauty is a registered trade mark for a coal slag media. The media has a very low Free Silica content, usually below 0.1% and is chemically inert. The media is manufactured in the USA by Reed Minerals. To contact Reed Minerals use the following,
Reed Minerals, Harsco Corp., P.O. Box 0515, Camp Hill, PA, 17001-0515,
Tel (717) 763-4200 or Fax (717) 763-6496.
Good Luck,
Ken l'Anson

Ken2Peen Services