Jack,

Thanks for your help so far.
I have some more questions about creation of %Intensity vs. Corner/Shot Radius Ratio Chart.

As usual, measurement laboratories make measurements at 7 to 9 depths to create stress profile on shot peened part.

Is it necessary to create part's stress profile to generate the data on this chart?

Or is it possible to make a single point-single depth measurement for data gathering?

What should minimum depth be for stress measurement?

Thanks in advance!


N. Hakan Karaaslan