I am working on intensity verification of shot peening process using mini Almen strips which are produced by Electronics Inc. I want to know the application procedure of mini strip for a given Almen intensity on a drawing. Is there any military or industrial specification reference for using mini Almen strips? Is there a limitaiton of use for mini Almen strips?
N. Hakan Karaaslan Metalworking Engineer GE Aviation