Jack, Socrates and John; thanks for your helpful messages.

Jack, I read the article. It is full of useful information. But I have two questions in my mind:

1-I understand that it is not necessary to attach mini strip to a standard strip holder as we do for standard strips. In this case, flattness of the surface that we attach mini strip doesn't take an important role. Should I take it like that?

2-Corelation work is done on a standard strip holder. This corelation work is done on a simple single almen holder fixture and expose to shot stream? or should we do it for different peening angles and intensity verification positions?

Thanks!
Hakan.


N. Hakan Karaaslan
Metalworking Engineer
GE Aviation

T +90 262 677 6044
E nevzat.karaaslan@ge.com

TUBITAK-MAM Teknoloji Serbest Bölgesi
41470, Gebze, Kocaeli, Turkey
GE Marmara Technology Center Muhendislik Hizmetleri Limited Sirketi