The knowledge base for the shot peening and blast cleaning industries
≡
About
The Website
Shot Peening
Library
Search the Library
Recently added articles
The Shot Peener
articles
Dr. David Kirk articles
Dr. John Cammett articles
Patents Granted
Patent Applications
Specifications
FAQs
Shot Peener of the Year
Wheelabrator History
Vacu-Blast History
Pangborn History
Jack's History Finds
Tools
Almen Saturation Curve Solver Program
Peening Coverage Predictor Program
Two-Strip Intensity Estimator
Program Request Form
Vibrator Screen Check Decal
Shot Peening Saturation Curve Practice Sheet
Roto-Flap Peening Saturation Curve Practice Sheet
Charts and graphs
Intensity as function of shot size for wheel peening
Sweco screen sizes for sand blasting and shot peening media
Vacu-Blast Engineering Specifications - Nozzle Performance
Buyer's Guide
Vendors
Products
Register company
Q & A Forum
News
Contact
Register
Log In
Home
Forums
General Discussion
Ask Dr. Peener
Plastic Media Blasting over a Shot Peened Surface
Forums
Active Threads
Previous Thread
Next Thread
Print Thread
Plastic Media Blasting over a Shot Peened Surface
#
959
01/02/13
09:05 PM
Joined:
Jan 2013
Posts: 1
E
ERayDurham
OP
Member
OP
ERayDurham
Member
E
Joined:
Jan 2013
Posts: 1
Is it OK to remove paint from a shot peened surface with plastic media? Do you know of any detrimental affects to the shot peened surface if the operator dwells too long in one location?
Copy Link to Clipboard
Entire Thread
Subject
Posted By
Posted
Plastic Media Blasting over a Shot Peened Surface
ERayDurham
01/02/13
09:05 PM
Re: Plastic Media Blasting over a Shot Peened Surface
Dave Barkley
01/04/13
02:02 PM
Moderated by
Socrates
Hop To
General Discussion ------
Shot Peening Process, Intensity...
Specifications
Equipment, Machines, Accessories
Abrasive Blast Cleaning Process
Media, Shot, Beads, etc.
Ask Dr. Peener
Print Thread
Switch to Flat Mode
Show Likes
Link Copied to Clipboard
View Profile
Private Message
Follow User
Forum Posts
Like Summary
Forum Rules
·
Mark All Read
Contact Us
·
Forum Help
·
Home
Sponsored by Electronics Inc. © 2025
Electronics Inc.
All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5