Previous Thread
Next Thread
Print Thread
#961 02/08/13 02:21 PM
Joined: May 2004
Posts: 2
P
Member
OP Offline
Member
P
Joined: May 2004
Posts: 2
Any special demand on ultraviolet light used with Peenscan or Fluoro-Finder?


Pether
Joined: May 1999
Posts: 202
Member
Offline
Member
Joined: May 1999
Posts: 202
You should be using a filtered black light at least 100 watts. The filter shall transmit wave lengths of between 3200 and 4000 angstrom units. The light intensity shall not be less than 1000 microwatts per square centimeter when meassured at a distance of 46-61 cm.