What can be a "good amps" range for Shot Peening round Steel Plates (3mmthick) at 46HRc with S230 Shots?

What can be called as higher & Lower limits for useful Shot Peening with the above process parameters.

Joined: Nov 2013
Posts: 10
B
Member
Offline
Member
B
Joined: Nov 2013
Posts: 10
You always want to study what compressive stress your part needs first. Then you do it.

Regarding the best Amp i prefer this instruction video:

https://www.youtube.com/watch?v=uMSV4OteqBE

One louder is sometimes better.


Shotpeen Engineer
Joined: Apr 2011
Posts: 49
Member
Offline
Member
Joined: Apr 2011
Posts: 49
Originally Posted By Blomberg
One louder is sometimes better.


"These go to eleven"

I recently saw a spec. (that will not be named) that gave a required various intensity ranges (i.e. 6-10A) and noted "A" as "Ampres" laugh

Merry Chirstmas Blomberg


Dave Barkley
EI SPT Director, Peening Preceptor & Product Engineer

Link Copied to Clipboard
Sponsored by Electronics Inc. © 2021 Electronics Inc. All Rights Reserved.
Powered by UBB.threads™ PHP Forum Software 7.7.5