Topic Options
#1077 - 01/17/14 09:39 AM comparison of cut wire sizes
Jack Champaigne Offline


Registered: 04/20/99
Posts: 325
Loc: Mishawaka, IN, USA
I have one more question regarding to shot peening with CCW 17. Do you have any experience about the CCW17 and the alternative usage of CCW 17 instead of CW14 and S110?

Top
#1078 - 01/17/14 09:40 AM Re: comparison of cut wire sizes [Re: Jack Champaigne]
Jack Champaigne Offline


Registered: 04/20/99
Posts: 325
Loc: Mishawaka, IN, USA
One of the determinates of shot size is its ability to fit into small filet or radius. If all of these sizes fit then the next determination is the ability (mass) of the media to achieve the intensity you desire. Generally speaking the size of the media will have very small (if any) difference on your part as long as you have the correct intensity and achieve full coverage.

Top
#1087 - 04/03/14 05:58 AM Re: comparison of cut wire sizes [Re: Jack Champaigne]
amit89 Offline
Member

Registered: 03/29/14
Posts: 25
dear Jack sir

can we use cut wire as pressure blast in nozzle?
can u have any experience of pressure blast with cut wire as blasting media?
any data of cut wire related to pressure and its flow rate in use of pressure blast.?

we made one machine pressure blast machine with use of cut wire. so do u have any data please suggest us.

thanks
amit89

Top
#1088 - 04/03/14 06:31 AM Re: comparison of cut wire sizes [Re: Jack Champaigne]
amit89 Offline
Member

Registered: 03/29/14
Posts: 25
dear Jack Sir
here below the data of cut wire to steel shot .

Cast Steel Shot Sizes and Equivalent Cut Wire Shot Sizes
Cast Steel US Standard Sieve Average Equivalent Cut
Size Ranges Diameter Wire Size
S-70 45 to 80 mesh 0.0117 CW 12*
S-110 40 to 50 mesh 0.0139 CW 14*
S-130 35 to 45 mesh 0.0165 CW 17*
S-170 30 to 40 mesh 0.0197 CW 17 CW 20*
S-190 25 to 35 mesh 0.0234 CW 20 CW 23*
S-230 20 to 30 mesh 0.0278 CW 23 CW 28*
S-280 18 to 25 mesh 0.0331 CW 28 CW 32*
S-330 16 to 20 mesh 0.0394 CW 32

thanks
amit89

Top
#1089 - 04/03/14 06:45 AM Re: comparison of cut wire sizes [Re: Jack Champaigne]
amit89 Offline
Member

Registered: 03/29/14
Posts: 25
sir
i have file but how can i upload this file.

please give way to upload so i ca give u.

u also contact me on mail id:- prajapati.99@gmail.com

thanks
amit89

Top


Sponsored by Electronics Inc. © 2020 Electronics Inc. All Rights Reserved.