#1081 - 03/17/14 06:21 PM Conditioned Cut Wire
tec Offline
Member

Registered: 11/01/13
Posts: 55
Is there a specification for the conditioning of cut wire to G1, G2 & G3? as nothing is defined in 2431/4

Top
#1097 - 04/08/14 11:06 AM Re: Conditioned Cut Wire [Re: tec]
Walter Offline



Registered: 05/03/99
Posts: 161
Loc: East Hartford, CT, USA
Look at these, I don't believe any will tell you how to condition the cut wire just what it should look like after it is performed. I would suggest you purchase your material pre-conditioned.

VDFI 8001, (DIN 8201-4), ISO 11124-1, AMS 2431-3, AMS 2431-8