#1170 - 09/21/15 06:39 AM Any "Good Amps" guide for Shot Peening?
Subhajyoti Offline
Member

Registered: 09/18/15
Posts: 7
Loc: India
Any "Good Amps" guide for Shot Peening?

What can be a "good amps" range for Shot Peening round Steel Plates (3mmthick) at 46HRc with S230 Shots?

What can be called as higher & Lower limits for useful Shot Peening with the above process parameters.

Top
#1308 - 12/04/17 07:06 AM Re: Any "Good Amps" guide for Shot Peening? [Re: Subhajyoti]
Blomberg Offline
Member

Registered: 11/15/13
Posts: 10
Loc: Sweden
You always want to study what compressive stress your part needs first. Then you do it.

Regarding the best Amp i prefer this instruction video:

https://www.youtube.com/watch?v=uMSV4OteqBE

One louder is sometimes better.
_________________________
Shotpeen Engineer

Top
#1309 - 12/04/17 10:59 AM Re: Any "Good Amps" guide for Shot Peening? [Re: Blomberg]
Dave Barkley Offline


Registered: 04/13/11
Posts: 49
Loc: USA
Originally Posted By Blomberg
One louder is sometimes better.


"These go to eleven"

I recently saw a spec. (that will not be named) that gave a required various intensity ranges (i.e. 6-10A) and noted "A" as "Ampres" laugh

Merry Chirstmas Blomberg
_________________________
Dave Barkley
EI SPT Director, Peening Preceptor & Product Engineer

Top


Sponsored by Electronics Inc. © 2021 Electronics Inc. All Rights Reserved.