Just recently received a customer request for LAT4-0214 spec. Many years in this industry and I have never encounter this spec before. Any help would greatly be appreciated

Top
#1188 - 11/18/15 07:38 AM Re: LAT4-0214 Spec [Re: Newf]
Florin Offline
Member

Registered: 11/17/15
Posts: 4
Loc: Canada
Hi the spec it a Liebherr specification, Glass Bead (Bright Shot) Peening for Bombardier