Hello,

I want to learn what do you assume as a lot (for an individual part) while intensity verification
A day?
A shift?
A week?
Or -Anything else?

Joined: May 1999
Posts: 199
Member
Offline
Member
Joined: May 1999
Posts: 199
A lot is defined as a part or group of parts that are shot peened one after another using the same machine without any changes to the set up.