I recommend the SJ-210 series by Mitutoyo. Its not cheap at about $2500 but it is a good piece of equipment. Computer connectivity is something I am not sure about, but it has its own LCD screen with data logging capability and roughness charts. Many of our aerospace customers also use this profilometer in their inspection areas.