Hi All,

Our customer drawing required shot peening with below shot:
SHOT SIZE 550
INTENSITY 12-14C
COVERAGE 200%
SHOT TYPE NON MAG

Non Mag shot is very new to me. Please help me explain "non mag shot" is made from what material?

Thank you and appreciate your support.

Top
#1323 - 01/30/18 07:43 AM Re: NON MAG SHOT [Re: donhan]
Dennis Scharer Offline


Registered: 01/16/07
Posts: 12
Loc: Adrian, Mi
Donhan

I would suggest going back to your customer and asking them to define the shot requirement. Maybe they could inform you of the media specification. 550 size is normally associated with cast steel shot which is magnetic. There is stainless cut wire, glass and ceramic peening media.


Edited by Dennis Scharer (01/30/18 07:44 AM)

Top
#1325 - 01/31/18 04:42 AM Re: NON MAG SHOT [Re: donhan]
donhan Offline
Member

Registered: 08/20/16
Posts: 14
Hi Dennis,

Thank you for your reply.

Top
#1523 - 03/10/21 09:06 PM Re: NON MAG SHOT [Re: donhan]
wendy zhang Offline
Member

Registered: 03/09/21
Posts: 2
Loc: 中国
Hi Donhan,
Non-mag shot should be made of 304 stainless steel, and non mag treatment on this materials.