I was just told that you do not have to be certified in general to perform a special process on aerospace components.

What is actually required?

Top
#1432 - 07/29/19 03:15 PM Re: Aerospace Qualification [Re: Rich]
Walter Online   content



Registered: 05/03/99
Posts: 161
Loc: East Hartford, CT, USA
Most Aerospace primes require you be both on their approved source list and Nadcap accredited. If the work is for overhaul and repair work you will need to be FAA and possibly EASA approved.