I am gearing up for an initial NADCAP Audit for Surface Enhancement. What are the typical nonconformance's encountered? And how would you address them?

Top
#1465 - 03/11/20 11:09 AM Re: Typical Nonconformances in a NADCAP Audit [Re: Rich]
Walter Online   content



Registered: 05/03/99
Posts: 167
Loc: East Hartford, CT, USA
Are you already registered for the audit and have access to https://www.eauditnet.com ? If not you will need to be.

Once you have access you can dig around and find the Surface Enhancement SE - Top NCRs,
and Supplier NCR Response Guidelines as well as the requirements and checklists. Make sure you download all the requirements and checklists for the processes you will be performing. Then perform your own internal audits to the checklists well in advance of the Nadcap audit. Correct any findings prior to the Nadcap audit. If you don't, you will fail the audit before you even start!

-Walter Beach
Peening Technologies of CT

Top
#1466 - 03/11/20 11:11 AM Re: Typical Nonconformances in a NADCAP Audit [Re: Rich]
Rich Offline
Member

Registered: 04/10/19
Posts: 18
Loc: Texas
I am registered and have access. I will look for this document. Thanks for the heads up.

Top
#1467 - 03/11/20 11:20 AM Re: Typical Nonconformances in a NADCAP Audit [Re: Rich]
Walter Online   content



Registered: 05/03/99
Posts: 167
Loc: East Hartford, CT, USA
Under Audit Criteria look for Surface Enhancement (AC7117)

Under Handbooks & Guides look for SE Audit Handbook

Under General Nadcap User Information / Audit Information look for Supplier NCR Response Guidelines.

Under 2018 Auditor Conferences Agendas and Presentations look for 2018 Auditor Conferences Agendas and Presentations >> NMSE - 2018 >> SE - Top NCRs

It does not appear that 2019 Top findings were added. You might want to look back at previous years as well.

Hope that helps,

Good Luck!

-Walter